To Hank, looking for 1234 Celadon.
--------------------------------------------------------
This Celadon recipe is from Ceramics Monthly, March 1982, Cone 9/10 and
sourced to Sandy Simon:

10 Kaolin
20 Whiting
30 Silica
40 Feldspar

ADD: 2% Red Iron Oxide

Dennis in Stafford, VA