search  current discussion  categories  glazes - cone 8-10 

^9-10 blue

updated sat 30 nov 96

 

Anne Yagoda on fri 15 nov 96

Here is the recipe for Seacrest Blue, as promised.

k-200 4833
flint 2016
whiting 1161
english china Clay 540
zinc 225
black iron oxide 270
rutile oxide 270

It doesn't add up to 10,000 grams but it works.

Happy glazing,
Anne in central NJ where it is winter too early!