Malone & Dean McRaine on wed 13 aug 97
Aloha. With all this discussion about the elusive Floating Blue, I'm
curious about trying it at ^9-10. Any suhggestions for modifying it for
this range?
Thanks
Dean McRaine
Ron Roy on fri 15 aug 97
Hi Dean,
Should be possible - which one do you want to start with - all GB, GB &
3124, all 3124, part GB and 3278 - or maybe 3124 and GB - the last one is a
possibility because the other two frits bring no Al2O3 and we have to add
alumina and silica to up the temperature.
>----------------------------Original message----------------------------
>Aloha. With all this discussion about the elusive Floating Blue, I'm
>curious about trying it at ^9-10. Any suhggestions for modifying it for
>this range?
>Thanks
>Dean McRaine
Ron Roy
Toronto, Canada
Evenings, call 416 439 2621
Fax, 416 438 7849
Studio: 416-752-7862.
Email ronroy@astral.magic.ca
Home page http://digitalfire.com/education/people/ronroy.htm
| |
|