search  current discussion  categories  techniques - slips 

another source for slip trailers

updated fri 28 feb 97

 

Christine Fennimore on tue 11 feb 97

Another good source for slip trailers that I discovered is in the fabric
paint department of a craft store. I picked up two sizes of plastic bottles
that are used to paint on fabric. The tips can be cut at varying widths and
have worked really well for both slip trailing and overglaze decoration.
Think I paid $.49 for the small ones and $.69 for the large ones.

Chris Fennimore
Native American Rights Fund
Boulder, Colorado
fennimor@spot.colorado.edu