search  current discussion  categories  glazes - ash 

ash glaze request

updated mon 30 sep 96

 

June Perry on sat 21 sep 96

Hi Everyone!

I'm looking for a recipe for a cone 10 mustard yellow matt ash glaze and also
a nice light to medium blue matt ash glaze. Does any one have either of these
that they may be willing to share? I have a good supply of various ashes and
would like to make good use of it!

Thanks!
June
EMail: Gurushakti@aol.com
or: juneperry@wave.net

Andrew S Lubow on sun 22 sep 96

How about a Tan one?

Mixed Wood Ash 25%
Custer Spar 32%
Dolomite 12%
EPK 10%
Flint 18%
Magnesium Carbonate 2%
Also Add:
Red Iron Oxide 2%
Rutile 3%
C.M.C. 1 tsp.

On Sat, 21 Sep 1996 10:07:45 EDT June Perry writes:
>----------------------------Original
>message----------------------------
>Hi Everyone!
>
>I'm looking for a recipe for a cone 10 mustard yellow matt ash glaze
>and also
>a nice light to medium blue matt ash glaze. Does any one have either
>of these
>that they may be willing to share? I have a good supply of various
>ashes and
>would like to make good use of it!
>
>Thanks!
>June
>EMail: Gurushakti@aol.com
>or: juneperry@wave.net
>