search  current discussion  categories  materials - clay 

avery slip

updated thu 25 apr 02

 

Stephen Sell on mon 6 oct 97

Fellow Clayart,
A friend fired a pot in my kiln this weekend that had Avery slip on it,
deep red, dry surface... The friend had no reciepe, got the slip at a
workshop...I've looked in the usual ceramic supply catalog with no luck. Any
body have a source for this stuff.

Thanks,

Stephen Sell / odaat2day@aol.com

Susan Goldstein on thu 9 oct 97

I believe that Avery is no longer available but there are nice substitutes
for it. If you would like some recipes please let me know.

Susan

Holly Keeney on wed 24 apr 02


I also need a recipe for Avery slip. Does someone out there have that
one? Thank you so much!
Holly