Karl P. Platt on fri 4 apr 97
I want to modify this statement a little
>>Suffice it to say that of all ofthe forms of Ba to have in a glaze, the presen
Actually, the worst case is a glassy glaze with high alkali and/or high
B2O3 and high BaO. Here the Ba is most weakly held than in any of its
crystalline forms.