>From: jennifer reilly
>
>Hi,
>
> I love purple glazes and I have found a lot of recipes containing
Barium. I would like to share my findings. In some glaze tests I
substituted stontium Carb for Barium(7-7.5ston to 1 barium). It didn't work
very well on bright glazes but on other ones it did.
>
>
>
>
>
>
>
>
>
>
>
>
>
>