Fred Hayward on mon 6 may 96
BARBROX@AOL.COM recently put out a request for a black matte glaze. I've been u
this one which Michelle Lowe posted here about 15 months ago. It's a nice deep
but when used over a white glaze is a deep midnight blue.
Crystalline Black ^6 ox
Dolomite 21
Gerstley Borate 5.25
Custer spar 15.75
Neph Syenite 26.5
Ball clay 21
Flint 10.5
Cobalt 6
Copper 6
Good luck!
Claudia
Maple Ridge B.C. in the Great Canadian South West!
| |
|