search  current discussion  categories  techniques - centering 

centering problems?

updated sat 31 aug 96

 

Lori Wilkinson on fri 23 aug 96

Having problems centering, especially larger amounts of clay? I was and
couldn't understand it. Thought the old wrist was about gone until I
thought to check the level of my wheel head. Come to find out the back of
my wheel had to be raised 1/4 of and inch. Duh! It was level when we
installed it about 5 years ago but the house or floor under it had settled.
I am almost too ambarassed to sign this.

Lori Wilkinson in Roswell NM