search  current discussion  categories  glazes - misc 

changing glaze to matte

updated thu 31 jul 97

 

Donna Hoff-Grambau on fri 11 jul 97

Hello! Recently someone sent me the following beautiful glaze called
Faux Lead cone ^04 range. I need to, however, make it more matte
instead of the glossy it is. Is there someone out there who has glaze
software that can help, I couldn't download the shareware for some
reason (time to figure out how).

Faux Lead

Frit 3110 30.6
Gerstley Borate 33
EPK 26
Flint 5
Wollastonite 3
Strontium Carbonate 2.5
Bentonite 2

Thanks.