Leona Stonebridge Arthen on mon 9 sep 96

Thanks to all those who helped with the unwanted chrome pink problem. Tom
Buck seemed to hit the nail on the head when he checked out my glaze and
suggested that the zinc level was too high for the chrome to be green.
There is no tin in any of my glazes so zinc must be the culprit. Thanks,
Tom!!! I have not been able to try your new formulation as I've been on
the road with the musical group I perform with and next week will be
visiting my dad in Illinois, not to mention working on the 300 pot order my
distributor just handed me... I'm sure I'll get to it someday.