Lisa or Ginny on mon 7 apr 97
What is Foundry Hill Creme?
--
Lisa Skeen
Living Tree Pottery
Greensboro, NC
YesIAmRU?
Email: lpskeen@nr.infi.net
Drew Montgomery on tue 8 apr 97
At 12:16 PM 4/7/97 EDT, you wrote:
>----------------------------Original message----------------------------
>What is Foundry Hill Creme?
Foundry Hill Creme is a smooth stoneware clay
0.212 Na2O
0.17 K2O
0.303 MgO
0.213 CaO
0.101 MnO
4.807 Al2O3
26.372 SiO2
1.384 P2O5
0.159 TiO2
0.24 Fe2O3
Drew Montgomery dcmontgomery@earthlink.net
| |
|