search  current discussion  categories  techniques - slips 

colorabia's 30 engobes

updated sat 31 may 97

 

Turfle, Susan A. on sat 10 may 97

I am posting for a friend -

I am currently preparing to test Colorabia's 30 engobes on 3 different
clay bodies by Standard Clay: #105 low fire white, #410 white
sculpture body, and #308 Brooklyn Red Stoneware at cone 6-8. These
are Italian made engobes generally used for cone 05-06 temps. Does
anyone have experience with these products at these higher temps?

Thanks in advance!

susan.turfle@jhuapl.edu