Here's a reliable Cone 10 glossy oribe that is a lovely jade green breaking
to blue where thick:
FLINT 24.66%
WHITING 21.83%
CUSTER (POTASH) FELDSPAR 30.12%
EPK 12.28%
TALC 7.6%
BONE ASH 1.07%
COPPER OXIDE BLACK 2.44%
We get lovely color in atmospheres from neutral to light reduction (heavy
reduction is not necessary).
A very reliable glaze!
Ellen Baker, Orion