Soliciting input or formulae for cone 4-6 white or porcelain casting bodies
for a project. Suggestions as to which kaolins orball clays one might use.
As usual, a broad diversification of particle sizes.

Ratio 50/50 between plastics and non plastics.

I have some ideas in mind and woudl be happy to post them with the above
suggestions from the list.

Please post me personally so as not to clog the list.

WIll reciprocate as usual.

TIA