Suzanne Storer on fri 13 jun 97
I'm in need of a cone 5 shiny black glaze. Anyone have one?
Thanks, Suzanne
Tony Hansen on sat 14 jun 97
Suzanne Storer wrote:
> I'm in need of a cone 5 shiny black glaze. Anyone have one?
A lot of people are using around 75% Alberta Slip with enough
frit or feldspar to melt it better and some added cobalt oxide
2-5% or iron:cobalt 8:1 or just black stain 3-7% (i.e. Mason
6666, 6600.
--
Tony Hansen, IMC thansen@mlc.awinc.com
J Rose Fine Pottery on thu 26 jun 97
Suzanne Storer wrote:
>
> ----------------------------Original message----------------------------
> I'm in need of a cone 5 shiny black glaze. Anyone have one?
> Thanks, Suzanne
Hi,
I'm very happy using ^5 High Gloss Black glaze from Laguna.
June Rosenberry
JRoseFine@Earthlink.net
| |
|