search  current discussion  categories  glazes - cone 4-7 

cone 6 crystalline glazes

updated sat 31 may 97

 

Joe Mann on wed 7 may 97

Sandi....

A good article is in the Dec.1975 Ceramic's Monthly by David Snare and
some good recipes that people that I know have fired successfully at cone
^6, again the hold should beat 1835 for three to four hours