Bacia Edelman on sat 17 may 97
Elizabeth Anderson wrote about a cone 7 bending in the sitter and witness
cone 6 not moving at all.
When this happened to me, I phoned Orton, 1-800/999-5442, asking for Ext. 22
and a cone expert named Dale Fronk. Describe to him whether your cones 6
are white (old) or tinted. I think the old 6's and 7's were differently
formulated. I know I tossed them after speaking with him. He will clear up
the problem for sure.
Good luck. Bacia Edelman Madison, WI
| |
|