>Steve here. I goofed a little. For a beautiful multi colored effect on
>your pieces, put 1/2 coats of copper sand then RED GREEN, not rainbow as I
>mentioned in my earlier post.
>
>Sorry hope I did not cause anyone problems..
>
>Steve
>
>