Kate Smith on mon 7 apr 97
Is Crocuss Martus - yellow simply yellow iron oxide?
stevemills on tue 8 apr 97
In message <3344DD71.483A@isd.net>, Kate Smith writes
>----------------------------Original message----------------------------
>Is Crocuss Martus - yellow simply yellow iron oxide?
Dear Kate, Hamer and Hamer Dictionary give Crocus Martis as anhydrous
ferrous sulphate FeSO4. I used it once when I ran out of Red Iron Oxide
to make my tenmoku and celadon glazes and saw no discernable difference
regards Steve.
--
Steve Mills
@Bath Potters Supplies
Dorset Close
Bath
BA2 3RF
UK
Tel:(44) (0)1225 337046
Fax:(44) (0)1225 462712
| |
|