Hi Oz,

What cone? Reduction or oxidation? Thanks.

Joyce
TooHot Mojave where Cindy Crawford just worked out in our small, local gym.

KEMPB on mon 13 may 96

To Joyce from "Hi Oz"
The Paul Davis Shino is a Cone 9-10 glaze, fired in reduction.
(I am amazed that Cindy Crawford hasn't been to see me working out in
my local Gym....not a pretty sight I can assure you)

Brian Kemp. Singapore