Susan Dispex is a defloculant used to defloculate
casting slip. We get from the UK. I am the local supplier
here in Port Elizabeth South Africa. My customers swear
by it saying that it is better than Sodium Silicate as it
also protects the mould. I use it together with Sodium
Silicate since it is so expensive. It works that way for me.
Hope this helps Ralph in PE SA.