search  current discussion  categories  techniques - slips 

fw: jasper slip-clay

updated mon 30 jun 97

 

laurie force on fri 27 jun 97

Hi Clayarters--
I just got this email on Jasper Slip. I've never tried to forward
attachments before; I hope it works.

Laurie Force
lforce@mesa5.mesa.colorado.edu


----------
> From: Eric Nedreberg
> To: lforce@mesa5.mesa.colorado.edu
> Subject: Jasper Slip-Clay
> Date: Wednesday, June 25, 1997 9:39 PM
>
> Dear Laurie,
>
> We were so swamped by the response from NCECA that we are still sending
out
> a few of the samples. You should by now have received via U.S. mail a
> letter with suggestions for use and some recipes, I apologize for not
> getting this letter to you at the same time you got the clay.
>
> In case you still have not received the letter, I have attached the Word
> Perfect file to this message. Let me know if you have any problems or
> questions.
>
> Thanks!!
>
> Eric Nedreberg
> General Manager, United Clays Huntingburg Works