Marvin S. Flowerman on thu 23 jan 97

Some of the senior students at Raritan Valley Community College in
Somerville, New Jersy are working on glaze development.

They are interested in obtaining recipies for LICHEN GLAZES, VOLCANIC GLAZES
AND ANY OTHER SPECIAL EFFECTS GLAZES that any of you fellow Clayartists can
recommend, together with firing details.

Many thanks.

Marvpots@AOL.Com

Ken Nowicki on fri 24 jan 97

In a message dated 97-01-23 14:20:56 EST, Marvin writes:


----------------------------Original message----------------------------
> Some of the senior students at Raritan Valley Community College in
> Somerville, New Jersy are working on glaze development.

> They are interested in obtaining recipies for LICHEN GLAZES, VOLCANIC
>GLAZES
> AND ANY OTHER SPECIAL EFFECTS GLAZES that any of you fellow >Clayartists
can
> recommend, together with firing details.

> Many thanks.

> Marvpots@AOL.Com

Marvin,

Check out the aritcle(s) written in Ceramics Monthly during the last 2 years
or so. I know Lana Wilson had at least one in there about her "lichen" glazes
she's developed. She's done extensive glaze testing in this area and has had
wonderful sucess. She also has a wonderful new book out called Ceramics:
Shapes and Surface which has some recipes and examples of her work, as well
as a ton of information regarding handouts, glaze development, formulas,
firing techniques, handouts for teachers. time management, creativity, etc.,
etc. Or you can contact her direct via snail mail or e-mail at:
Lana Wilson
465 Hidden Pines Lane
Del Mar, CA 92014
(619) 755-3940
email: lwilson@ucsd.edu

Lana is a former professor of mine and a wonderful, generous lady. I'm sure
she would be helpful in directing you to some sources for your request. (On a
side note, she is one of the lecturers & panelists at this year's NCECA in
Las Vegas... if you are attending, you may want to make sure you catch her
panel/lecture.)
Good luck!

Ken

Wendy Hampton on sat 25 jan 97

Hi Marvin,
There are a lot of special effect glazes on Glazebase. Go to
http:/apple.sdsu.edu/ceramicsweb/galzedatabase.html. You will have scads of
glazes to use!
Wendy

Salvador Acosta on sat 25 jan 97

Dear Marvin,
What cone and atmosphere will the senior students be firing to?


> Some of the senior students at Raritan Valley Community College in
> Somerville, New Jersy are working on glaze development.
>
> They are interested in obtaining recipies for LICHEN GLAZES, VOLCANIC GLAZES
> AND ANY OTHER SPECIAL EFFECTS GLAZES that any of you fellow Clayartists can
> recommend, together with firing details.
>
> Many thanks.
>
> Marvpots@AOL.Com

Karen Gringhuis on fri 31 jan 97

Marv - WHAT CONE? If C/6 or 9/10 and if you don't already have a glaze
w/ around 35% Mag Carb, RSVP & I'll send. Karen Gringhuis