BabsDeluxe on wed 22 oct 97

I've used gold leaf for years under the second or third layer of a low fire
clear glaze (cone 06). It makes for a floating effect , kinda like gold leaf
in glass, (oops that's what it is..lol) Great for beads , tops of container ,
ect . Good luck
BabsDeluxe@aol.com

"keeper of the listing" hehe
http://members.aol.com/BabsDeluxe/ceramics.html
or htm
thank you everyone for lending your FAQ's !

Beth Elliott on thu 23 oct 97

Hi Basbs & All
Do you use real gold leaf or composition leaf? Seems like composition leaf
would probably burn out in an 06 fire??
Gracias
Beth in LA