search  current discussion  categories  materials - misc 

gold leaf/eucalyptus oil

updated fri 24 oct 97

 

Many Mused on thu 9 oct 97

you could probably use clove oil instead, and a good glass fusing supply
should have one or the other.
The oil burns away- it is just a temporary adhesive for the leaf.