DaveDDP on sun 11 may 97
Have a sprung arch kiln-18 cu. ft. interior space -want to fire to cone
10. Four ports. Present burners too big. Does anyone have construction
details for Alfred type burners that would work? Plan on using propane so
need oriface size.
reply to DaveDDP@AOL
"Rafael Molina-Rodriguez (Rafael Molina-Rodriguez)" on sun 8 jun 97
Dave :
Plans for Alfred pipe burner can be found on page 202 of "The Kiln Book" by
Frederick L. Olsen. ISBN # 0-8019-7071-7.
Good luck!
Rafael
rmr3431@dcccd.edu
>>> DaveDDP 05/11/97 09:59am >>>
----------------------------Original message----------------------------
Have a sprung arch kiln-18 cu. ft. interior space -want to fire to cone
10. Four ports. Present burners too big. Does anyone have construction
details for Alfred type burners that would work? Plan on using propane so
need oriface size.
reply to DaveDDP@AOL
| |
|