search  current discussion  categories  kilns & firing - misc 

in search of salt firing glazes

updated sat 30 nov 96

 

Michele Dorff on wed 30 oct 96

I've done a few reduction firings in a salt kiln and am interested in finding
a few more glazes to try. I've been firing to ^1. Any recipes you'd like to
share? Thanks!

Michele Dorff (mdorff@coe.edu)
Coe College
Cedar Rapids, IA

"Rafael Molina-Rodriguez (Rafael Molina-Rodriguez)" on fri 1 nov 96

Michele:

Is that a typo or do you really do reduction firings in a salt kiln to ^ 1? Did
you mean to type ^ 10?

If it's ^ 10 I'll post some glazes soon.

Rafael
Rmr3431@dcccd.edu

>>> Michele Dorff 10/30/96 09:37pm >>>
----------------------------Original message----------------------------
I've done a few reduction firings in a salt kiln and am interested in finding
a few more glazes to try. I've been firing to ^1. Any recipes you'd like to
share? Thanks!

Michele Dorff (mdorff@coe.edu)
Coe College
Cedar Rapids, IA