Marcia Selsor on sun 2 feb 97

I have only used ITC on shelves in soda firing. works great.
can't say for wood, but I think soda is more caustic.
Marcia in Montana
George VanOstrand wrote:
>
> ----------------------------Original message----------------------------
> I notice The coating ITC is getting very good press on clayart. Has anyone
> used it for coating on shelves. I fire with wood and soon with soda and
> wonder how it would work. Do glaze drips come off easily?
> George VanOstrand
> gvanostr@julian.uwo.ca
> London, Ontario

--