search  current discussion  categories  kilns & firing - coatings 

itc over greenpatch

updated mon 30 jun 97

 

KDrescherg on thu 12 jun 97

Has anyone used ITC over greenpatch? They told me on the phone that they
are incompatable, yet it seems that ITC works like a miracle cure over a
variety of different surfaces.

Greenman
drescherg@aol.com