Malone & Dean McRaine on sun 5 oct 97

Aloha;
I'm moving into gas ^10 reduction firing after many years of electric ^10
oxidation. I have a friend firing small clay/glaze tests for me in his ^10
reduction firings and it's very helpful. Local conditions are similar and
our firing will be similar as well-also helpful to keep initial glazes
faults limited to small pieces.