Talbott on thu 14 aug 97

Fran... Thanks for the information on the kiln wash... I would have never
known why the stuff was so caked up unless you had posted to Clayart... I
found out that the bad batch of wash was sent out without a suspender being
added to it...

Thanks ....Marshall
----------------------------Original message----------------------------

Axner received a bad batch of Lee's Kiln Wash. They were working on
replacements when the UPS strike occurred. Call Howard Axner or any one
working in Customer Service and let them know the problems you are
experiencing. We did and received a very good reception and quick response.

Good Luck. Fran, Tin Barn Pottery at Manassas Clay, Virginia


1ST ANNUAL CLAYARTERS' GALLERY - NAPLES, MAINE (Summer 1997)
http://fmc.utm.edu/~dmcbeth/cag/naples.htm
2nd Annual Clayarters' Gallery details will be forth coming!!!

Celia & Marshall Talbott, Pottery By Celia, Route 114, P O Box 4116,
Naples, Maine 04055-4116,(207)693-6100 voice and fax,(call first)
WBS Live Chat Room, Sat Nites 10 PM EDT & Sun Afternoons at
1 PM EDT Private Room: Clayarters E-MAIL: clupus@ime.net