Is there a low fire [cone 010] clear glaze? If so ,could you give me the
formula or tell me what to purchase. Thanks. Jay Landis
Beverly Cohen on sun 30 mar 97
>----------------------------Original message----------------------------
>Is there a low fire [cone 010] clear glaze? If so ,could you give me the
>formula or tell me what to purchase. Thanks. Jay Landis
>
Jay,
I wasn't aware that there were glazes that fired cooler than cone 06, so
I will be interested in seeing any response to this, too. I was always
under the impression that anything cooler than 06 would be classified as
an overglaze, such as a luster, fired gold, etc. It's what I love about
ClayArt--all the information here just for the having.