Eleanora Eden on sun 24 nov 96

Hi Sharon and All,

I don't pretend to have the last word on the subject of oven-wareability,
but I have always just used a stoneware body for a lowfire ovenwre body
and I have never had any trouble myself nor complaints.

I bisc at cone 04 and glaze at 06 and don't do anything differently with
it than for my regular ware.


Eleanora