search  current discussion  categories  wanted/for sale - misc 

maria's work

updated thu 31 jul 97

 

Sylvia See on mon 14 jul 97

Joyce: Maria painted on bisqued pottery, with mason stains and water. I
glazed the pieces with a commercial clear cone 05 in electric kiln. Maria
prefers cone 06 oxidation, but I couldn't get my hands on any in time
before she left so settled for cone 05. They turned out beautifully, the
glaze was sprayed very carefully as I was terrified I would ruin her work
and many of the pieces belonged to other potters. She prefers cone 06
oxidation, as she believes the colors remain truer at that temp.