MRS DIANE S ZUBRICK on mon 8 apr 96

I read with interest about the presentation of Mitsubishi's Precious
Metal Clay at the NCECA. Could someone tell me how to order this
material? Does anyone have a copy of the handout that they are
willing to share or know where I can write for more information?

Thanks in advance,

Diane Schwob Zubrick
Applecreek Pottery
Centerville, Ohio

Jean Lehman on tue 9 apr 96


Hi, Diane.

The North American dealer for PMC is:

Rio Grande Gems and Findings
6901 Washington NE
Albuquerque, NM 87109
1-800-443-6766

I am sure they will be happy to send information. The paper I have says
that a quarter pound is the minimum order for the gold PMC and at the time
it was printed was $225.40 for one package of that amount!!!

If anyone is couragous enough to try this, I HOPE you will give us a report.

Good luck!!!

Jean



>----------------------------Original message----------------------------
>I read with interest about the presentation of Mitsubishi's Precious
>Metal Clay at the NCECA. Could someone tell me how to order this
>material? Does anyone have a copy of the handout that they are
>willing to share or know where I can write for more information?
>
>Thanks in advance,
>
>Diane Schwob Zubrick
>Applecreek Pottery
>Centerville, Ohio