Craig Martell on sat 27 sep 97
Buenos Dias:
I've been meaning to send this for a bit.
I talked to Christie at Georgies Ceramic and Clay Co. in Portland, Or. about
the new boron product, Cadycal 100. Some of you probably remember that the
analysis only added up to 77.95% and there was no Loss on Ignition given etc.
Anyway, Christie didn't have much to add, only that Cadycal is a real new
product but has shown promise as being much more reliable than Gerstley
Borate or Colemanite. It is being mined in California by The Feldspar Corp.
Their website is and their e-mail address is
, and their fax # is (770)392-8670. Those interested can
hopefully obtain more details on the material by making contact with the Co.
adios, Craig Martell-Oregon
Ron Roy on mon 29 sep 97
Hi Graig,
I sent them an email about 8 days ago and nothing back yet - very strange -
are you sure you are not making all this up?
>I've been meaning to send this for a bit.
>
>I talked to Christie at Georgies Ceramic and Clay Co. in Portland, Or. about
>the new boron product, Cadycal 100. Some of you probably remember that the
>analysis only added up to 77.95% and there was no Loss on Ignition given etc.
>
>Anyway, Christie didn't have much to add, only that Cadycal is a real new
>product but has shown promise as being much more reliable than Gerstley
>Borate or Colemanite. It is being mined in California by The Feldspar Corp.
>Their website is and their e-mail address is
>, and their fax # is (770)392-8670. Those interested can
>hopefully obtain more details on the material by making contact with the Co.
>
>adios, Craig Martell-Oregon
Ron Roy
93 Pegasus Trail
Scarborough,Canada
M1G 3N8
Evenings, call 416 439 2621
Fax, 416 438 7849
Studio: 416-752-7862.
Email ronroy@astral.magic.ca
Home page http://digitalfire.com/education/people/ronroy.htm
| |
|