Carol Jackaway's comments on adding a "DAB" (good word, Carol) of glaze at
the joints really works. Use of a "Dab" of frit mixed in the slurry that is
used for the attaching "Glue" works also. Give Nils Lou credit for that one.
He saved me by passing that one on to me. It works. It is especially good
with porcelain, especially slip cast porcelain.

John Rodgers