Sherry mcDonald Stewart on thu 17 apr 97

Has anyone used this tile press? I would like some feedback from those
who have. I design small tiles in relief, and normally make molds and
pour slip to pick up the fine details, but I am considering a tile
press. Anyone???

Yost Tile Co. on tue 22 apr 97

>----------------------------Original message----------------------------
>Has anyone used this tile press? I would like some feedback from those
>who have. I design small tiles in relief, and normally make molds and
>pour slip to pick up the fine details, but I am considering a tile
>press. Anyone???

I like the press for low relief tiles up to four inch square. I have broken
the handles twice and North Star replaced the parts without question. Bob
Creighton is the gentleman that I dealt with and he is a good guy.
good luck making tile, bob