notation for reduction or oxidation

updated wed 30 apr 97

 

The Shelfords on fri 25 apr 97

Would those posting recipes please be sure to note not only the cone, but
also whether it is ox. or red.? I can figure it out if it is called copper
red or rutile blue, but it's not always obvious. Thanks!

Veronica