search  current discussion  categories  kilns & firing - misc 

oxidation at end of firing schedule

updated mon 30 sep 96

 

Talbott on thu 26 sep 96

I am firing cone 10 reduction (a gas kiln)--I would like to get info from
some of you on your firing schedule--do you go into oxidation at the end of
the firing cycle prior to shut down???--If you use an oxy-probe (which I
do) then can you tell me how strongly that you reduce.(ie: .5/.6/.7 on your
multimeter)--any "top secret" info that you give to me will be most
appreciated..Thank you clayarters... I have learned a lot since I started
this...Marshall

Marshall Talbott
Pottery By Celia
Route 114
P.O. Box 4116
Naples, Maine 04055-4116
(207)693-6100 voice and fax
clupus@ime.net