P. F. Shelor on fri 13 dec 96
Would someone kindly repost the recipe for the oxidation red glaze that I saw
a couple of weeks ago?
Thanks in advance.
Andrew S Lubow on sat 14 dec 96
Was it this one?
Here is an Ox Blood Red that I've used in the past. Apply it HEAVILY for
the best results.
Gerstly Borate 54.88%
Talc 14.63%
Flint 30.49%
=====
100%
+ Red Iron Oxide 21.95%
On Fri, 13 Dec 1996 08:50:34 EST "P. F. Shelor" writes:
>----------------------------Original
>message----------------------------
>Would someone kindly repost the recipe for the oxidation red glaze
>that I saw
>a couple of weeks ago?
>
>Thanks in advance.
>
Fred Hayward on sun 15 dec 96
Andrew S Lubow wrote:
>
> ----------------------------Original message----------------------------
> Was it this one?
>
> Here is an Ox Blood Red that I've used in the past. Apply it HEAVILY for
> the best results.
>
> Gerstly Borate 54.88%
> Talc 14.63%
> Flint 30.49%
> =====
> 100%
> + Red Iron Oxide 21.95%
What cone???
Andrew S Lubow on mon 16 dec 96
Sorry for the confusion it's a Cone 6 glaze.
On Sun, 15 Dec 1996 11:15:22 EST Fred Hayward
writes:
>----------------------------Original
>message----------------------------
>Andrew S Lubow wrote:
>>
>> ----------------------------Original
>message----------------------------
>> Was it this one?
>>
>> Here is an Ox Blood Red that I've used in the past. Apply it HEAVILY
>for
>> the best results.
>>
>> Gerstly Borate 54.88%
>> Talc 14.63%
>> Flint 30.49%
>> =====
>> 100%
>> + Red Iron Oxide 21.95%
>
>What cone???
>
| |
|