search  current discussion  categories  kilns & firing - raku 

peuter raku

updated thu 31 jul 97

 

Toni Hall on mon 28 jul 97

Teruhiko,
About your peuter raku question, I have used a Duncan glaze called
Peuter, and it does well in raku. Also I have used Tsuya's Mistake (can't
remember where I got this glaze), and it has a rather metal/peuter finish.

Tsuya's Mistake (Raku)

Copper Carb 50
Frit 3110 50
Total 100

Good luck, Toni in NM