Pat Everson on thu 23 oct 97
Phoenix # 8
Hi all,
Well I am calling this # 8 but I am not sure if I sent # 7, and am thinking
that I jumped right from # 5 to # 7. If anyone is saving these would you
please let me know? (I have saved them and don't have a #6.)
Also, I will be off line for 2 weeks starting 10/27. Can someone tell me how
to put clayart on hold for that time so my mailbox doesn't overflow?
Now for the kiln.
Since last time we have gone up with the walls through course 15. Course 12
seemed to be a crucial course but there was no diagram for it so we just did
what seemed to make sense. We are only using mortar now for leveling.
problems: none in particular
concerns: next arch, level, remembering to rowlock, plum (make sure those
walls are going up straight)
Pat
anxious to see New Mixico...leaving Monday
pjeve2@aol.com