search  current discussion  categories  materials - plaster 

plaster bat molds/left over plaster

updated fri 28 feb 97

 

Marcia Selsor on wed 26 feb 97

To add to this, when I am making plaster molds (i persoanlly don't use
plaster bats) I always have toilet paper tubes nearby for pouring the
excess plaster into. They can be carved into rolling stamps.
Marcia in Montana

Ric Swenson wrote:
>
> ----------------------------Original message----------------------------
> >----------------------------Original message----------------------------
> >Need to jump in here and make some corrections about plaster.
> >
nutes, then pour over a sharp edge to break any entrapped
> >air.
> >
> >Jonathan
> >
> >
> >
> >Jonathan Kaplan
> >Ceramic Design Group Ltd./Production Services
experience at Bennington Potters.)
>
> As I think of it...also..."never" pour left over plaster down a sink drain!
> Make sculptures of it!.... quickly!
>
> Enjoy!
>
> Ric Swenson, Bennington, Vermont

--
Marcia Selsor
http://www.imt.net/~mjbmls/
mjbmls@imt.net