Paul Monaghan on wed 16 jul 97
Friends,
Does anyone do or know of someone who can repair porcelain clock faces?
I have a customer on our website http://www.web2u.com "Bill's Clock
Shop" who occassionally needs porcelain clock faces repaired. I may be
able to send the proper person some work in the future.
--
Paul J. Monaghan email: paul@web2u.com
WEB2U Productions --- http://www.web2u.com
The "COOLEST" Site on the WEB
"The Computer Secrets are hidden at http://www.web2u.com/secret"
"HOMO CLAYARTUS" is alive at http://www.web2u.com/clayart
James L Bowen on thu 17 feb 00
-------------------
There are many methods of ceramic repair available to owners, collectors and
dealers of valuable antique and contemporary ceramics. Some are virtually
invisible to the naked untrained eye. Buyer beware thet there are an ever
increasing number of unscrupulous sellers out there. A good black light =
will