Richard mahaffey on mon 12 may 97
Hi,
I am posting this for a student of mine at Tacoma Community College. He
is starting a series of tests based on Bob Kavanagh's article in January
1996 Ceramics Monthly. He asks:
1. Is this slip galze a once fire process?
2. Should he put teh s-2 glaze over the pot after the slip is applied, or
is it only mixed with the white slip as a white undercoat?
3. Which glaze application technique is best dipping, spray, pour,
brushing?
If Bob Kavanagh is on the list or if anyone knows how to reach him I would
appreciate the information. You can email me at:
rmahaffe@linknet.kitsap.lib.wa.us
or
rmahaffe@tcc.tacoma.ctc.edu
Thank's in advance.
Rick Mahaffey Tacoma, Washington, USA
| |
|