search  current discussion  categories  glazes - cone 04-06 

recipe for terra-cotta low fire slip

updated fri 24 oct 97

 

Larry Tague on sun 12 oct 97

Hi everyone, I am looking for a recipe for a low fire terra-cotta slip. I'm
with the understanding that the main ingredient is Red Art. Are there other
ingredients? I can't seem to find much information on this subject. TIA
Carol Tague
megtague@msn.com

DIANA PANCIOLI, ASSOC. PROF. on tue 14 oct 97

Please describe more precisely what you are looking for--a terra cotta
colored slip for terra cotta clay at Cone 04? Maybe I can help.

Larry Tague on wed 15 oct 97

I am looking for a terra cotta slip recipe that I can make from redart. I have
had several responses that say, "yes you can make it from redart", but I need
a little guidance. TIA Carol (megtague@msn.com)

----------
From: Ceramic Arts Discussion List on behalf of DIANA PANCIOLI, ASSOC. PROF.
Sent: Tuesday, October 14, 1997 7:48 AM
To: Multiple recipients of list CLAYART
Subject: Re: recipe for terra-cotta low fire slip

----------------------------Original message----------------------------
Please describe more precisely what you are looking for--a terra cotta
colored slip for terra cotta clay at Cone 04? Maybe I can help.