search  current discussion  categories  glazes - cone 4-7 

reglazing cone 6-8 ox

updated thu 31 jul 97

 

P. F. S. on tue 15 jul 97

If I want to reglaze a pot with a glossy surface using the same glaze
again, what additive should I use to improve adherence of the glaze
for the second firing.

Boyd on wed 16 jul 97

PFS,

Thin and strain the glaze, fire up the air brush and apply thin coats and
dry it with a hair dryer. OR---Let the glaze settle out, siphon off the top and
apply the thick stuff any way you wish. I'm sure you'll hear of a dozen other
methods but this is the way I approach it when I have to reglaze.

Boyd
Iron River MI

At 01:35 PM 7/15/97 EDT, you wrote:
>----------------------------Original message----------------------------
>If I want to reglaze a pot with a glossy surface using the same glaze
>again, what additive should I use to improve adherence of the glaze
>for the second firing.
>
>
http://www.freeyellow.com/members/boyd/index.html